In the quenched and tempered condition, ASTM 4140 steel has good strength, toughness, wear resistance and fatigue resistance.Therefore,ASTM 4140 steel is usually delivered in the pre-hardened condition(PH) with hardness 28-34HRC.
ASTM 4140
Chemical requirements:
Standard | Grade | C | Si | Mn | P | S | Cr | Ni | Mo |
ASTM A29 | 4140 | 0.38-0.43 | 0.15-0.35 | 0.75-1.00 | ≤ 0.035 | ≤ 0.04 | 0.8-1.1 | – | 0.15-0.25 |
| 42CrMo4 |
|
|
|
|
|
|
|
|
1.7225 | |||||||||
JIS G4105 | SCM440 | 0.38-0.43 | 0.15-0.35 | 0.6-0.85 | ≤ 0.035 | ≤ 0.04 | 0.9-1.2 | – | 0.15-0.30 |
GB 3077 | 42CrMo | 0.38-0.45 | 0.17-0.37 | 0.5-0.80 | ≤ 0.035 | ≤ 0.035 | 0.9-1.2 | – | 0.15-0.25 |
BS 970 | EN19 | 0.35-0.45 | 0.15-0.35 | 0.5-0.80 | ≤ 0.035 | ≤ 0.035 | 0.9-1.5 | – | 0.2-0.40 |
Tensile requirements:
Grade | Tensile Strength | Yield Strength | Elongation | Reduction of Area | Impact Charpy-V |
4140 | ≥1100Mpa | ≥950Mpa | ≥12% | ≥45% | ≥80 |