Standard Specification for ASTM A959-2004 SS310

UNS 310
AISI S31000
Standard ASTM A959-2004
Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
Classification Austenitic stainless steel
Introductions Compared with 309 stainless steel, it has higher strength and oxidation resistance at higher temperatures. It is used in the manufacture of heat exchange equipment, furnace components, combustion chambers, welding filler metal, gas turbine components, incinerators, co-flow heat exchangers and rollers for roll bottom furnaces.

 

310 Chemical Element Content (%)
Constituent C Si Mn P S Cr Ni
Min 24 19
Max 0.25 1.5 2 0.045 0.03 26 22

 

China Taiwan, China Japan Korea America The International Standard Organization Germany France European standard Russia United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical grade GOST BS EN/BS
20Cr25Ni20 S31020 SUH 310 SUH 310 STR 310 310 S31000 X15CrNi 25-21 X15CrNiSi 25-20 1.4841 Z15CNS 25-20 X15CrNi 25-20 1.4845 20Х25Н20С2 310S31
(2Cr25Ni20)